Recovery of nickel from spent nickel-cadmium batteries using a direct reduction process

3Citations
Citations of this article
13Readers
Mendeley users who have this article in their library.

Abstract

Most nickel is produced as Ferro-Nickel through a smelting process from Ni-bearing ore. However, these days, there have been some problems in nickel production due to exhaustion and the low-grade of Ni-bearing ore. Moreover, the smelting process results in a large amount of wastewater, slag and environmental risk. Therefore, in this research, spent Ni-Cd batteries were used as a base material instead of Ni-bearing ore for the recovery of Fe-Ni alloy through a direct reduction process. Spent Ni-Cd batteries contain 24wt% Ni, 18.5wt% Cd, 12.1% C and 27.5wt% polymers such as KOH. For pre-treatment, Cd was vaporized at 1024K. In order to evaluate the reduction conditions of nickel oxide and iron oxide, pre-treated spent Ni-Cd batteries were experimented on under various temperatures, gas-atmospheres and crucible materials. By a series of process, alloys containing 75 wt% Ni and 20 wt% Fe were produced. From the results, the reduction mechanism of nickel oxide and iron oxide were investigated.

Cite

CITATION STYLE

APA

Shin, D. J., Joo, S. H., Wang, J. P., & Shin, S. M. (2015). Recovery of nickel from spent nickel-cadmium batteries using a direct reduction process. Archives of Metallurgy and Materials, 60(2), 1365–1370. https://doi.org/10.1515/amm-2015-0132

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free