Effect of Cooling Rate and Slag Modification on the Copper Matte in Smelting Slag

18Citations
Citations of this article
14Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The amount of copper flash smelting slag has increased during the recent years along with an increasing slag-to-metal ratio. During slag tapping, some copper sulfide is mechanically entrained. As a result, it is necessary to recover copper matte from the slag by suitable methods. At present, the most common way is slow, controlled cooling in a transfer ladle. However, research on the detailed effects of slow cooling and the function of slag modification is rare. This paper described experiments that were performed at different cooling rates (0.5, 1.5, 3, and 7 °C/min), with and without additive. A detailed characterization of the copper-rich phase and its particle size was subsequently made using SEM-EDS micrographs and image analysis software. With a decrease in cooling rate, the particle size of the copper-rich matte phase became larger. The addition of gypsum and carbon as a slag modifier affected the size of the copper-rich phase slightly, and its chemical composition was modified compared with the experiments without additive.

Cite

CITATION STYLE

APA

Gao, X., Chen, Z., Shi, J., Taskinen, P., & Jokilaakso, A. (2020). Effect of Cooling Rate and Slag Modification on the Copper Matte in Smelting Slag. Mining, Metallurgy and Exploration, 37(5), 1593–1601. https://doi.org/10.1007/s42461-020-00274-x

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free