Compositionally tunable ternary Bi2(Se1-xTex)3 and (Bi1-ySby)2Te3 thin films via low pressure chemical vapour deposition

18Citations
Citations of this article
22Readers
Mendeley users who have this article in their library.

Abstract

The inherently rapid ligand substitution kinetics associated with the novel and chemically compatible precursors, [MCl3(EnBu2)3] (M = Sb, Bi; E = Se, Te), enable CVD growth of ternary Bi2(Se1-xTex)3 and (Bi1-ySby)2Te3 thin films with very good compositional, structural and morphological control, for the first time. X-ray diffraction data follow Vegard's law and Raman bands shift linearly with the atom substitutions, indicating very well-distributed solid solutions.

Cite

CITATION STYLE

APA

Benjamin, S. L., De Groot, C. H., Gurnani, C., Hawken, S. L., Hector, A. L., Huang, R., … Stenning, G. B. G. (2018). Compositionally tunable ternary Bi2(Se1-xTex)3 and (Bi1-ySby)2Te3 thin films via low pressure chemical vapour deposition. Journal of Materials Chemistry C, 6(29), 7734–7739. https://doi.org/10.1039/c8tc01285g

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free