Evolution of LiNi0.8Mn0.1Co0.1O2 (NMC811) Cathodes for Li-Ion Batteries: An In Situ Electron Paramagnetic Resonance Study

10Citations
Citations of this article
25Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The rapid voltage and capacity fade of the otherwise promising Ni-rich layered LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode are the primary obstacles to its successful commercialization in lithium-ion batteries (LIBs). Here, in situ electrochemical electron paramagnetic resonance (EPR) spectroscopy is employed to gain insight into the cation redox behavior of the NMC811 cathode during the cell charge/discharge process. Different oxidation states of Ni ions are detected by variations in the signal of the EPR spectra. Ex situ studies of NMC811 at different SOC levels also confirm changes in the local Mn-Ni environment. A comparison of in situ studies on fresh and cycled NMC811 electrodes demonstrates that the fundamental redox processes remain unchanged upon cycling of the material. Finally, dissolved Mn and Co ions from the bulk are found using ex situ EPR characterization of the cycled cathode and separator. The dissolution of these metal ions can accelerate the degradation of the entire battery.

Cite

CITATION STYLE

APA

Wang, B., Redondo, E., Le Fevre, L. W., Brookfield, A., McInnes, E. J. L., & Dryfe, R. A. W. (2025). Evolution of LiNi0.8Mn0.1Co0.1O2 (NMC811) Cathodes for Li-Ion Batteries: An In Situ Electron Paramagnetic Resonance Study. Journal of Physical Chemistry C, 129(16), 7667–7676. https://doi.org/10.1021/acs.jpcc.5c00275

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free