The P110 steel specimens were subjected to ultrasonic cavitation erosion in different compositions of drilling muds and surfactant additive. The test procedure was based on ASTM-G-32 standard recommendations. API 5CT-P110 steel is used for pipes in oil and gas industry. The harsh environment and high velocity of flows poses corrosive and erosive threat on materials used there. The composition of drilling fluid influences its rheological properties and thus intensity of cavitation erosion. The erosion curves based on weight loss were measured.
Cite
CITATION STYLE
Kmieć, M., Karpiński, B., & Szkodo, M. (2016). Cavitation Erosion of P110 Steel in Different Drilling Muds. Advances in Materials Science, 16(2), 57–67. https://doi.org/10.1515/adms-2016-0009