Method of preparation for high-purity nanocrystalline anhydrous cesium perrhenate

5Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

This paper is devoted to the preparation of high-purity anhydrous nanocrystalline cesium perrhenate, which is applied in catalyst preparation. It was found that anhydrous cesium perrhenate with a crystal size <45 nm can be obtained using cesium ion sorption and elution using aqueous solutions of perrhenic acid with subsequent crystallisation, purification, and drying. The following composition of the as-obtained product was reported: 34.7% Cs; 48.6% Re and <2 ppm Bi; <3 ppm Zn; <2 ppm As; <10 ppm Ni; < 3 ppm Mg; <5 ppm Cu; <5 ppm Mo; <5 ppm Pb; <10 ppm K; <2 ppm Na; <5 ppm Ca; <3 ppm Fe.

Cite

CITATION STYLE

APA

Leszczyńska-Sejda, K., Benke, G., Ciszewski, M., Malarz, J., & Drzazga, M. (2017). Method of preparation for high-purity nanocrystalline anhydrous cesium perrhenate. Metals, 7(3). https://doi.org/10.3390/met7030096

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free