Spontaneous growth of cabi4ti4o15 piezoelectric crystal using mixed flux agents

6Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

The bismuth layer-structured ferroelectrics (BLSFs) materials have potential for high-temperature piezoelectric applications. Among these piezoelectric materials, the CaBi4Ti4O15 (CBT) piezoelectric ceramic with a high decomposition temperature of about 1250◦C attracts a lot of attention. Achieving a CBT single crystal is a significant way to improve its piezoelectric properties. For this purpose, the flux system for growing CBT crystal was explored in this study. The optimum flux composition ratio was found to be PbO:B2O3:CBT = 3:3:1 in mol%, where the PbO–B2O3 mixtures were used as a flux system. Millimeter size flake-shaped CBT crystals were obtained using the spontaneous growth process for the first time. The relationship between the crystal structure and flake growth habit was analyzed. In addition, the bandgap was evaluated by the combination of transmittance spectrum and first-principle calculations. Besides, the piezoelectric property was predicted from the perspective of polyhedral distortion, which indicated the potential of CBT crystal for piezoelectric applications.

Cite

CITATION STYLE

APA

Fan, M., Wu, G., Yu, F., Li, L., Li, Y., Cheng, X., & Zhao, X. (2020). Spontaneous growth of cabi4ti4o15 piezoelectric crystal using mixed flux agents. Crystals, 10(8), 1–10. https://doi.org/10.3390/cryst10080698

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free