Investigating the effect of post weld heat treatment on corrosion properties of explosive bonded interface of AA5083/AA1050/SS 321 tubes

46Citations
Citations of this article
15Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The corrosion behavior and microstructural changes in explosively welded AA5083/AA1050/SS 321 multilayer tubes after heat treatment were studied. Heat treatment were performed in 350 and 450 °C for 6 and 8 h. Microscopic results indicated significant changes in the thickness and concentration of alloying elements in locally melting zone with heat treatment temperature. According to electrochemical tests results at samples interfaces, by increasing the temperature and time of the heat treatment process, the energy stored due to explosive welding is reduced, the difference in the concentration of aluminum related to steel in the interface layer decreases, and the corrosion rate (current density) and electrical charge transfer decrease.

Cite

CITATION STYLE

APA

Shargh, S. F., Saadat, A., Najafi, A., Gharehshiran, M. R. K., & Khalaj, G. (2020). Investigating the effect of post weld heat treatment on corrosion properties of explosive bonded interface of AA5083/AA1050/SS 321 tubes. Materials Research Express, 7(3). https://doi.org/10.1088/2053-1591/ab8095

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free