Abstract
Evidence of structural fatigue has been detected at the surface of discharged Lix[Mn2]O4 spinel electrodes in (4 V) Li/Lix[Mn2]O4 cells. Under nonequilibrium conditions, domains of tetragonal Li2[Mn2]O4 coexist with cubic Li[Mn2]O4, even at 500 mV above the thermodynamic voltage expected for the onset of the tetragonal phase. The presence of Li2[Mn2]O4 on the particle surface may contribute to some of the capacity fade observed during cycling of Li/Lix[Mn2]O4 cells. © 1998 The Electrochemical Society, Inc.
Cite
CITATION STYLE
Thackeray, M. M., Shao-Horn, Y., Kahaian, A. J., Kepler, K. D., Skinner, E., Vaughey, J. T., & Hackney, S. A. (1998). Structural fatigue in spinel electrodes in high voltage (4 V) Li/LixMn2O4 cells. Electrochemical and Solid-State Letters, 1(1), 7–9. https://doi.org/10.1149/1.1390617