Solubility product of VN in austenite of high Cr heat resistant steel

16Citations
Citations of this article
15Readers
Mendeley users who have this article in their library.

Abstract

Dissolved V in austenite of 7%Cr-0.4%V-0.09% steel (hereinafter, % means mass%) was measured and the solubility product of VN was determined as follows: log([%V][%N])=4.38-8 436/T where T is the absolute temperature in K. The solubility product obtained is 3 to 5 times larger than those in the literature and about one order larger than that for iron. The decrease in the activity coefficient of nitrogen due to the presence of Cr and V in the experimental steel is responsible for the increase in the solubility product of VN.

Cite

CITATION STYLE

APA

Tamura, M., Iida, H., Esaka, H., & Shinozuka, K. (2003). Solubility product of VN in austenite of high Cr heat resistant steel. ISIJ International, 43(11), 1807–1813. https://doi.org/10.2355/isijinternational.43.1807

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free