Effect of Barium in Porcelain on Bonding Strength of Titanium-Porcelain System

14Citations
Citations of this article
7Readers
Mendeley users who have this article in their library.

Abstract

The bonding strength to titanium, thermal expansion, and bending strength of glassy porcelain containing barium of 5, 10, and 15 mass% were estimated and compared with those of barium-free porcelain, to estimate the effect of barium content on bonding strength to titanium. The three different glassy porcelains containing barium were made by melting at 950°C. The bonding strength of a commercial porcelain to titanium increased with the addition of barium. Bending strength and thermal expansion were not affected by the barium content. Therefore, the addition of barium to porcelain is effective for strengthening the bonding of porcelain to titanium.

Cite

CITATION STYLE

APA

Oka, K., Hanawa, T., Kon, M., Lee, H. H., Kawano, F., Tomotake, Y., … Asaoka, K. (1996). Effect of Barium in Porcelain on Bonding Strength of Titanium-Porcelain System. Dental Materials Journal, 15(2), 111–120. https://doi.org/10.4012/dmj.15.111

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free