In this investigation, A356 aluminium alloy has been prepared by different routes viz. gravity casting, rheo pressure die casting (RPDC) and RPDC with T6 heat treatment. X-ray diffraction studies of these samples have been done in the scanning range of 20-90°. X-ray peak broadening analysis has been used to estimate the crystallite size and lattice stain, in all the samples. The sample prepared by RPDC with T6 treatment has comparatively smaller crystallite size and lesser lattice strain than gravity cast and RPDC samples.

Cite

CITATION STYLE

APA

Mishra, S. K., Roy, H., Lohar, A. K., Samanta, S. K., Tiwari, S., & Dutta, K. (2015). A comparative assessment of crystallite size and lattice strain in differently cast A356 aluminium alloy. In IOP Conference Series: Materials Science and Engineering (Vol. 75). Institute of Physics Publishing. https://doi.org/10.1088/1757-899X/75/1/012001

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free