A simple one-step anodising method for the synthesis of ordered porous anodic alumina

13Citations
Citations of this article
11Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

Porous anodic alumina (PAA) has been produced on aluminium substrate by single-step anodising at 50 V in 0.3 M oxalic acid at 15°C for 60 min. The highly ordered pore and cell structure was achieved by subjecting the PAA to oxide dissolution treatment in a mixture of chromic and phosphoric acids. The nanostructure prior and post-oxide dissolution treatment was examined under scanning electron microscope. It was found that the oxide dissolution treatment improves the regularity of the cell and pore structure significantly. Uniform closely packed honeycomb structure of PAA is obtained. The uniformities of pore diameter and interpore distance are also enhanced. Compared to the PAA prior treatment, it was noticed that the pore diameter of the post-treatment PAA increases. © 2014 Taylor and Francis Group, LLC.

Cite

CITATION STYLE

APA

Voon, C. H., Derman, M. N., Hashim, U., Ahmad, K. R., & Ho, L. N. (2014). A simple one-step anodising method for the synthesis of ordered porous anodic alumina. Journal of Experimental Nanoscience, 9(2), 106–112. https://doi.org/10.1080/17458080.2011.630151

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free