Gold Extraction from a Refractory Sulfide Concentrate by Simultaneous Pressure Leaching/Oxidation

17Citations
Citations of this article
50Readers
Mendeley users who have this article in their library.

Abstract

Most gold deposits occur associated with sulphides like pyrite and arsenopyrite; thus, precious metal dissolution is possible by oxidizing auriferous sulfide concentrate using simultaneous pressure oxidation and cyanidation. The effectiveness of this process of extraction can be influenced by the temperature, cyanide (NaCN) concentration, and oxygen pressure. In this study, we conducted experiments to characterize the effects on gold extraction of ores using a range of sodium cyanide concentrations (1–8 g/L), temperatures (40–75 °C), and oxygen pressures (0.5–1.1 MPa). Characterization of the ores showed that pyrite and quartz were the main minerals present in the concentrate. The best results in terms of the highest extraction of Au were obtained with an oxygen pressure of 0.5 MPa, 6 g/L sodium cyanide, and a temperature of 75 °C, along with a constant stirring speed of 600 rpm. These conditions allowed for approximately 95% gold extraction in 90 min.

Cite

CITATION STYLE

APA

Soto-Uribe, J. C., Valenzuela-Garcia, J. L., Salazar-Campoy, M. M., Parga-Torres, J. R., Tiburcio-Munive, G., Encinas-Romero, M. A., & Vazquez-Vazquez, V. M. (2023). Gold Extraction from a Refractory Sulfide Concentrate by Simultaneous Pressure Leaching/Oxidation. Minerals, 13(1). https://doi.org/10.3390/min13010116

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free