Abstract

The consumption of water with fluoride concentration higher than 1.5 mg/L (WHO recommended limit) is recognized to cause serious diseases. Fluoride removal from natural contaminated waters is a worldwide priority for more than 200 million people. The octacalcium phosphate (OCP), a mineralogical precursor of bio-apatite, is here tested as a fluoride remover. A new two-step method for the synthesis of OCP is proposed; it consists of 1) synthesis of brushite from calcium carbonate and phosphoric acid and, 2) subsequent hydrolysis of brushite. Fluoride removal experiments were performed in batch-mode using 200 mg of OCP in 50 ml solutions with different initial concentrations of fluoride (from 40 to 140 mg/L). Most of fluoride is removed within the first two hours, whereas the WHO limit of 1.5 mg/L is reached within a minimum of 3 hours for a starting Fconcentration of 40 mg/L, and in about 12 hours for a starting F-concentration of 80 mg/L. One gram of OCP can remove up to 26 mg of fluoride. The pH of the solution after the treatment is within the range of drinking water. XRD characterization of the solid phases, before and after the experiments, indicates that OCP transforms into fluorapatite via Fremoval from solution.

Cite

CITATION STYLE

APA

Idini, A., Dore, E., Fancello, D., Ghiglieri, G., & Frau, F. (2019). Dissolved fluoride removal by OCP, a precursor of apatite. In E3S Web of Conferences (Vol. 98). EDP Sciences. https://doi.org/10.1051/e3sconf/20199809012

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free