Characteristics of ADI ductile cast iron with single addition of 1.56% Ni

4Citations
Citations of this article
13Readers
Mendeley users who have this article in their library.

Abstract

The results of examinations of microstructure and an analysis of its impact on selected mechanical properties of austempered ductile iron (ADI) were presented in the paper. The ADI was produced from the ductile iron containing 1.56% Ni only alloying addition. The effect of the austempering time and temperature on the microstructure and mechanical properties of the examined cast iron was considered. Constant conditions of austenitizing were assumed and six variants of the austempering treatment were adopted. The studyof mechanical properties included a static tensile test, Charpy impact strength test and Brinellhardness measurement. This work complements the knowledge about alloying additions effect on microstructure and mechanical properties of ADI and focuses on the impact of a single alloying element (Ni).

Cite

CITATION STYLE

APA

Mrzygłód, B., Kowalski, A., Olejarczyk-Wozenska, I., Giȩtka, T., & Głowacki, M. (2017). Characteristics of ADI ductile cast iron with single addition of 1.56% Ni. Archives of Metallurgy and Materials, 62(4), 2273–2280. https://doi.org/10.1515/amm-2017-0335

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free