Abstract

Journal of the Korean Ceramic Society Vol. 45, No. 9, pp. 518~523, 2008. ... †Corresponding author : Do Kyung Kim E-mail : dkkim@kaist.ac.kr Tel : +82-42-869-4151 Fax : +82-42-869-3310 ... Mechanical Properties of Chemical - Vapor - Deposited Silicon Carbide using a ...