Modeling pitting corrosion by means of a 3D discrete stochastic model

  • Van der Weeën P
  • Zimer A
  • Pereira E
 et al. 
  • 5

    Readers

    Mendeley users who have this article in their library.
  • N/A

    Citations

    Citations of this article.

Abstract

Pitting corrosion is difficult to detect, predict and design against. Modeling and simulation can help to increase the knowledge on this phenomenon as well as to make predictions on the initiation and progression of it. A cellular automaton based model describing pitting corrosion is developed based on the main mechanisms behind this phenomenon. Further, a sensitivity analysis is performed in order to get a better insight in the model , after which the information gained from this analysis is employed to estimate the model parameters by means of experimental time series for a metal electrode in contact with different chloride concentrations. © 2014 Elsevier Ltd.

Author-supplied keywords

  • A. Steel
  • B. Modeling studies
  • C. Pitting corrosion

Get free article suggestions today

Mendeley saves you time finding and organizing research

Sign up here
Already have an account ?Sign in

Find this document

Authors

  • P. Van der Weeën

  • A.M. Zimer

  • E.C. Pereira

  • L.H. Mascaro

  • O.M. Bruno

  • B. De Baets

Cite this document

Choose a citation style from the tabs below

Save time finding and organizing research with Mendeley

Sign up for free