Highly conductive and stretchable conductors fabricated from bacterial cellulose

238Citations
Citations of this article
276Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

Advanced materials that can remain electrically conductive under substantial elastic stretch and bending have attracted extensive interest recently owing to their broad application potentials, particularly for flexible electronics. Here, we have developed a simple and inexpensive method to fabricate highly conductive and stretchable composites using bacterial cellulose (BC) pellicles as starting materials, which can be produced in large amounts on an industrial scale via a microbial fermentation process. The prepared pyrolyzed BC (p-BC)/polydimethylsiloxane (PDMS) composites exhibit a high electrical conductivity of 0.20-0.41 S cm 1, which is much higher than conventional carbon nanotubes and graphene-based composites. More importantly, the p-BC/PDMS composites that combine high stretchability with high conductivity show great electromechanical stability. Even after 1000 stretching cycles at the maximum strain of 80%, the resistance of the composites increased by only 10%. The resistance increased slightly (4%) after 5000 bending cycles with a maximum bending radius of 1.0 mm. © 2012 Nature Japan K.K. All rights reserved.

Cite

CITATION STYLE

APA

Liang, H. W., Guan, Q. F., Zhu, Z. Z., Song, L. T., Yao, H. B., Lei, X., & Yu, S. H. (2012). Highly conductive and stretchable conductors fabricated from bacterial cellulose. NPG Asia Materials, 4(6). https://doi.org/10.1038/am.2012.34

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free