A three-dimensional reticular macro-porous SiOC ceramics structure, made of spherical agglomerates, has been thermally characterized using a freestanding sensor-based 3\omega 3 ω method. The effective thermal conductivity of the macro-porous SiOC ceramics, including the effects of voids, is found to be 0.041\,\hbox { W}\cdot \hbox { m}^{-1}\cdot \hbox { K}^{-1}0.041 W · m - 1 · K - 1 to 0.078\,\hbox { W}\cdot \hbox { m}^{-1}\cdot \hbox { K}^{-1} 0.078 W · m - 1 · K - 1 at room temperature, comparable with that of alumina aerogel or carbon aerogel. These results suggest that SiOC ceramics hold great promise as a thermal insulation material for use at high temperatures. The measured results further reveal that the effective thermal conductivity is limited by the low solid-phase volume fraction for the SiOC series processed at the same conditions. For SiOC ceramics processed under different pyrolysis temperatures, the contact condition between neighboring particles in the SiOC networks is another key factor influencing the effective thermal conductivity. © 2013 Springer Science+Business Media New York.
CITATION STYLE
Qiu, L., Li, Y. M., Zheng, X. H., Zhu, J., Tang, D. W., Wu, J. Q., & Xu, C. H. (2014). Thermal-conductivity studies of macro-porous polymer-derived SiOC ceramics. International Journal of Thermophysics, 35(1), 76–89. https://doi.org/10.1007/s10765-013-1542-8
Mendeley helps you to discover research relevant for your work.