Fatigue tests were carried out with as-rolled and heat-treated Si-Mn-Cr-Mo martensite-ferrite dual-phase steels at room temperature in air and 3.5% NaCl solution. The effects of duplex microstructural morphologies, martensite contents and environmental conditions on fatigue stress-life, cyclic deformation behavior, fatigue crack initiation and near-threshold fatigue crack growth were investigated. The influence of prestrain and ageing on fatigue threshold was also studied.
CITATION STYLE
Wang, Z. G., & Ai, S. H. (1999). Fatigue of martensite-ferrite high strength low-alloy dual phase steels. ISIJ International, 39(8), 747–759. https://doi.org/10.2355/isijinternational.39.747