A sol–gel technique was successfully employed in creating pure and W-substituted zinc ferrite, with nominal compositions of ZnFe2−2xWxO4 (0.0 ≤ x ≤ 0.15). For the purposes of investigating the physical and chemical properties of the generated powders, several analytical techniques were used. In TEM images of all the compositions, mixed-shaped particles (cubic, spherical, and hexagonal) were observed. The crystallite size decreases from 82 nm (x = 0.0) to 32 nm (x = 0.15) with an increase in the W doping contents in the ZnFe2O4 lattice. The microstrain increases with increasing W doping content. Furthermore, the surface area of pure ZnFe2O4, 0.05 W-ZnFe2O4, 0.10 W-ZnFe2O4, and 0.15 W-ZnFe2O4 NPs were calculated as being 121.5, 129.1, 134.4 and 143.2 m2 g−1, respectively, with a mesoporous pore structure for all ferrite samples. The calculated BJH pore size distribution was within the range of 160 to 205 Å. All W-doped ZnFe2O4 samples show H-M loops with paramagnetic characteristics. The magnetization (M) directly increases by increasing the applied field (H) without achieving saturation up to 20 kA/m. For comparison, the magnetization at 20 kA/m gradually decreases with increasing W doping content. Among all the synthesized samples, the 0.15 W-ZnFe2O4 NPs demonstrated the highest sensitivity towards acetone gas at 350 °C.

Cite

CITATION STYLE

APA

Al-Enizi, A. M., Abd-Elkader, O. H., Shaikh, S. F., Ubaidullah, M., Abdelkader, M. O., & Mostafa, N. Y. (2022). Fabrication and Characterization of W-Substituted ZnFe2O4 for Gas Sensing Applications. Coatings, 12(9). https://doi.org/10.3390/coatings12091355

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free