We investigated effects of storage temperature and duration on release of antimony (Sb) and bisphenol A (BPA) from 16 brands of polyethylene terephthalate (PET) drinking water bottles in China. After 1-week storage, Sb release increased from 1.88-8.32 ng/L at 4 °C, to 2.10-18.4 ng/L at 25°C and to 20.3-2604 ng/L at 70°C. The corresponding releases for BPA were less at 0.26-18.7, 0.62-22.6, and 2.89-38.9 ng/L. Both Sb and BPA release increased with storage duration up to 4-week, but their releasing rates decreased with storage time, indicating that Sb and BPA release from PET bottles may become stable under long term storage. Human health risk was evaluated based on the worst case, i.e., storage at 70 °C for 4-week. Chronic daily intake (CDI) caused by BPA release was below USEPA regulation, Sb release in one brand exceeded USEPA regulated CDI (400 ng/kg bw/d) with values of 409 and 1430 ng/kg bw/d for adult and children. © 2014 Elsevier Ltd. All rights reserved.

Cite

CITATION STYLE

APA

Fan, Y. Y., Zheng, J. L., Ren, J. H., Luo, J., Cui, X. Y., & Ma, L. Q. (2014). Effects of storage temperature and duration on release of antimony and bisphenol A from polyethylene terephthalate drinking water bottles of China. Environmental Pollution, 192, 113–120. https://doi.org/10.1016/j.envpol.2014.05.012

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free