The aim of this study was to test the hypothesis that there is no difference in the fluoride release behavior of resin-reinforced glass ionomer cements before or after fluoride recharge. The materials were divided into 5 groups: 2 resin-reinforced glass ionomer cements used for attaching orthodontic bands, that is, group FOB (Fuji Ortho Band) and group MCB (Multi-Cure Glass Ionomer Orthodontic Band Cement); 2 resin-reinforced glass ionomer cements and a composite used for bonding orthodontic brackets, that is, group OGLC (Ortho Glass LC), group FOLC (Fuji Ortho LC), and group TXT (Transbond XT), respectively. Fluoride release was measured during a 60-day period by using selective ion electrodes connected to an ionic analyser. After 4 weeks, the samples were exposed to 0.221% sodium fluoride solution. The results showed that cements achieved a maximum fluoride release 24 h after initial setting. No statistically significant differences were observed between groups FOB and OGLC regarding the amount of released fluoride following fluoride recharge from day 31 to day 36 (p>0.05). In conclusion, FOB and OGLC cements showed a higher capacity of capturing and releasing fluoride compared to the other cements studied.
CITATION STYLE
dos Santos, R. L., Pithon, M. M., Vaitsman, D. S., de Souza Araújo, M. T., de Souza, M. M. G., & Nojima, M. G. da C. (2010). Long-term fluoride release from resin-reinforced orthodontic cements following recharge with fluoride solution. Brazilian Dental Journal, 21(2), 98–103. https://doi.org/10.1590/s0103-64402010000200002
Mendeley helps you to discover research relevant for your work.