Zn0.95Ni0.05O has been synthesized by mixing 5% mol of NiO into ZnO using solid state reaction and high-speed shaker mill method. The samples were sintered at 900 °C with holding time for 2, 4 and 8 hours. Crystal structure, electrical and magnetic properties of Zn0.95Ni0.05O were characterized by using XRD, I-V, C-V and VSM. XRD results showed that variation of holding time does not change the structure of ZnO and no other secondary phase observed. The value of lattice parameters (a and c) tends to decrease proportionally to the holding time. The Intensity value changes and the peak shifted to a higher 2θ angle due to holding time variation. In general, the conductance of Zn0.95Ni0.05O decreases and the magnetic properties decrease also as the holding time is increased.
CITATION STYLE
Ginting, M., Aryanto, D., Kurniawan, C., Sari, A. Y., Subhan, A., Sudiro, T., … Sebayang, K. (2017). Effects of Sintering Holding Time on the Structural, Electrical and Magnetic Properties of Zn0.95Ni0.05O. In IOP Conference Series: Materials Science and Engineering (Vol. 202). Institute of Physics Publishing. https://doi.org/10.1088/1757-899X/202/1/012033
Mendeley helps you to discover research relevant for your work.