Sustainable civil construction in the future, besides having low energy consumption and greenhouse gas emissions, must also adopt the principle of reusing wastes generated in the production chain that impact the environment. The aluminum production chain includes refining using the Bayer process. One of the main wastes produced by the Bayer process that has an impact on the environment is fly ash. Geopolymers are cementitious materials with a three-dimensional structure formed by the chemical activation of aluminosilicates. According to studies, some are proving to be appropriate sources of Al and Si in the geopolymerization reaction. The research reported here sought to assess the possibility of reusing fly ash characteristic of the operational temperature and pressure conditions of Bayer process boilers in geopolymer synthesis. Geopolymerization reaction was conducted at an ambient temperature of 30°C, and the activator used was sodium hydroxide (NaOH) 15 molar and sodium silicate (Na2SiO3) alkaline 10 molar. Fly ash and metakaolin were used as sources of Al and Si. XRD, XRF, and SEM Techniques were used for characterizing the raw materials and geopolymers. As a study parameter, the mole ratios utilized followed data from the literature described by Davidovits (year), so that the best results of the geopolymer samples were obtained in the 2.5 to 3.23 range. Resistance to mechanical compression reached 25 MPa in 24 hours of curing and 44 MPa after 28 days of curing at ambient temperature.

Figures

  • Table 1: Compositions formulated using fly ashes and metakaolin for obtaining geopolymers.
  • Table 2: Molar concentration and proportions of the activating solution.
  • Figure 1: XRD of kaolin, of metakaolin, and of fly ash.
  • Figure 2: Distribution of the size particles for fly ash and metakaolin.
  • Figure 3: XRD of geopolymers 2, 7, and 9 before and after synthesis.
  • Table 3: Chemical composition in % of ash and of metakaolin.
  • Figure 4: Compressive Strength (MPa) of the geopolymers.
  • Figure 5: Scanning electron microscopy (SEM): (a) Geopolymer 9 increase 500x; (b) Geopolymer 4 increase 500x.

References Powered by Scopus

3786Citations
3142Readers
Get full text

A review on the utilization of fly ash

2346Citations
2785Readers
Get full text
1527Citations
1487Readers
Get full text

Cited by Powered by Scopus

This article is free to access.

0Citations
2Readers

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Cite

CITATION STYLE

APA

Brito, W. S., Silva, A. L. M. F., Santa, R. A. A. B., Svensson, K., Da Silva Souza, J. A., Pöllmann, H., & Riella, H. G. (2018). An Assessment of Reuse of Light Ash from Bayer Process Fluidized Bed Boilers in Geopolymer Synthesis at Ambient Temperature. Advances in Materials Science and Engineering, 2018. https://doi.org/10.1155/2018/1287243

Readers over time

‘18‘19‘20‘21‘22‘23‘2402468

Readers' Seniority

Tooltip

PhD / Post grad / Masters / Doc 6

75%

Professor / Associate Prof. 1

13%

Researcher 1

13%

Readers' Discipline

Tooltip

Engineering 8

80%

Energy 1

10%

Chemistry 1

10%

Save time finding and organizing research with Mendeley

Sign up for free
0