At the southeastern part of Sweden, old art and crystal waste glass has been identified as a hazardous waste due to high weight concentrations of Pb (32.398%), Cd (0.085%), and As (1.976%). The reduction-melting technique was used to investigate the extraction of these trace elements from powder waste glass of particle size < 1 mm. Following a factorial design technique, the experimental results of the reduction-melting method showed that 99.9% of Pb, 100% of Cd, and 99% of As could be extracted. For a batch of 10 g powder waste glass, the found experimental and theoretical optimum operating conditions were 1100 °C of melting temperature, 5 g of Na2CO3, 2 g of carbon, and 120 min of melting time. The reduction-melting method displayed promising results which might help in recycling the extracted trace elements and glass compared to the current used solution of landfilling as hazardous wastes.
CITATION STYLE
Jani, Y., & Hogland, W. (2017). Reduction-melting extraction of trace elements from hazardous waste glass from an old glasswork’s dump in the southeastern part of Sweden. Environmental Science and Pollution Research, 24(34), 26341–26349. https://doi.org/10.1007/s11356-017-0243-4
Mendeley helps you to discover research relevant for your work.