Abstract

A thin BN interphase is applied on BNNTs surface to tailor the interfacial bonding between BNNTs and SiC matrix in hierarchical SiCf/SiC composites. The thickness of BN interphase ranging from 10 to 70 nm can be optimized by chemical vapor deposition after BNNTs are in situ grown on SiC fiber surface. Without BN interphase, the fracture toughness of hierarchical SiCf/SiC composites can be impaired by 13.6% due to strong interfacial bonding. As long as BN interphase with 30–45 nm thickness is applied, the interfacial bonding can be optimized and fracture toughness of hierarchical composites can be improved by 27.3%. It implies that tailoring BNNTs/matrix interface by depositing a layer of BN interphase is in favor of activating energy dissipation mechanisms at nanoscale induced by BNNTs.

Cite

CITATION STYLE

APA

Zhu, G., Feng, Q., Yang, J., Hu, J., Wang, H., Xue, Y., … Dong, S. (2019). Effect of BNNTs/matrix interface tailoring on toughness and fracture morphology of hierarchical SiCf/SiC composites. Journal of Advanced Ceramics, 8(4), 555–563. https://doi.org/10.1007/s40145-019-0338-0

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free