Evaporation of Fe and Cr from induction-stirred austenitic stainless steel. Influence of the inert gas pressure

23Citations
Citations of this article
13Readers
Mendeley users who have this article in their library.

Abstract

In vacuum metallurgy, one of the purposes is the reduction (or at least the accurate prediction) of the evaporation losses. It is well known that the addition of an inert gas in a vacuum furnace increases the recondensation of the volatile elements and then reduces the evaporation losses. We may define the pressure P1/2 required to halve the evaporation rate. The objective of this study is a theoretical and experimental evaluation of P1/2 in the case of an austenitic stainless steel, and the analysis of the parameters which influence this value. The experimental programme was carried out on an austenitic stainless steel to determine the net flux of evaporation from a well-mixed liquid in an ambient pressure of argon ranging from 0.03 to 133 Pa. P1/2=30 Pa is estimated from the experimental curve. The mechanisms of volatilization have been modeled using both a system based and a mechanistic approach, and the calculation of the pressure P1/2 gives respectively 45 and 90 Pa. The numerical simulations (mechanistic approach) emphasize the strong expansion of the vapor from the high density regions close to the liquid surface. The macroscopic velocity of the vapor decreases as the argon pressure in the chamber increases since the average frequency of collision with the argon atoms increases.

Cite

CITATION STYLE

APA

Bellot, J. P., Duval, H., Ritchie, M., Mitchell, A., & Ablitzer, D. (2001). Evaporation of Fe and Cr from induction-stirred austenitic stainless steel. Influence of the inert gas pressure. ISIJ International, 41(7), 696–705. https://doi.org/10.2355/isijinternational.41.696

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free