Mechanical properties of Mg-Y-Zn alloy processed by equal-channel-angular extrusion

34Citations
Citations of this article
21Readers
Mendeley users who have this article in their library.

Abstract

Fine-grained WZ73 magnesium alloy with the grain size of 1.6 μm was produced by Equal-Channel-Angular Extrusion. The material exhibited tensile yield strength of 293 MPa, tensile strength of 350 MPa and relatively large elongation of 18% at room temperature. The yield strength was almost unchanged up to 473 K. In addition, large superplastic elongation of over 300% was obtained at a temperature of 673 K.

Cite

CITATION STYLE

APA

Watanabe, H., Mukai, T., Kamado, S., Kojima, Y., & Higashi, K. (2003). Mechanical properties of Mg-Y-Zn alloy processed by equal-channel-angular extrusion. Materials Transactions, 44(4), 463–467. https://doi.org/10.2320/matertrans.44.463

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free