Abstract

High-performance biological materials such as nacre, spider silk or bone have evolved a staggered microstructure consisting of stiff and strong elongated inclusions aligned with the direction of loading. This structure leads to useful combinations of stiffness, strength and toughness, and it is therefore increasingly mimicked in bio-inspired composites. The performance of staggered composites can be tuned; for example, their mechanical properties increase when the overlap between the inclusions is increased. However, larger overlaps may lead to excessive tensile stress and fracture of the inclusions themselves, a highly detrimental failure mode. Fracture of the inclusions has so far only been predicted using highly simplified models, which hinder our ability to properly design and optimize engineered staggered composites. In this work, we develop a new failure criterion that takes into account the complex stress field within the inclusions as well as initial defects. The model leads to an 'optimum criterion' for cases where the shear tractions on the inclusions is uniform, and a 'conservative' criterion for which the tractions are modelled as point forces at the ends of the overlap regions. The criterion can therefore be applied for a wide array of material behaviour at the interface, even if the details of the shear load transfer is not known. The new criterion is validated with experiments on staggered structures made of millimetre-thick alumina tablets, and by comparison with data on nacre. Formulated in a non-dimensional form, our new criterion can be applied on a wide variety of engineered staggered composites at any length scale. It also reveals new design guidelines, for example high aspect ratio inclusions with weak interfaces are preferable over inclusions with low aspect ratio and stronger interfaces. Together with existing models, this new criterion will lead to optimal designs that harness the full potential of bio-inspired staggered composites. © 2012 The Author(s) Published by the Royal Society. All rights reserved.

References Powered by Scopus

The conflicts between strength and toughness

2990Citations
N/AReaders
Get full text

Freezing as a path to build complex composites

1760Citations
N/AReaders
Get full text

Materials become insensitive to flaws at nanoscale: Lessons from nature

1715Citations
N/AReaders
Get full text

Cited by Powered by Scopus

Structure and mechanics of interfaces in biological materials

571Citations
N/AReaders
Get full text

Impact-resistant nacre-like transparent materials

337Citations
N/AReaders
Get full text

Overcoming the brittleness of glass through bio-inspiration and micro-architecture

304Citations
N/AReaders
Get full text

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Cite

CITATION STYLE

APA

Barthelat, F., Dastjerdi, A. K., & Rabiei, R. (2013). An improved failure criterion for biological and engineered staggered composites. Journal of the Royal Society Interface, 10(79). https://doi.org/10.1098/rsif.2012.0849

Readers' Seniority

Tooltip

PhD / Post grad / Masters / Doc 54

61%

Researcher 23

26%

Professor / Associate Prof. 12

13%

Readers' Discipline

Tooltip

Engineering 48

61%

Materials Science 25

32%

Chemistry 3

4%

Physics and Astronomy 3

4%

Save time finding and organizing research with Mendeley

Sign up for free