Laser Lift-Off of the Sapphire Substrate for Fabricating Through-AlN-Via Wafer Bonded Absorption Layer Removed Thin Film Ultraviolet Flip Chip LED

5Citations
Citations of this article
8Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

In this study we report chip fabrication process that allows the laser lift-off of the sapphire substrate for the transfer of the GaN based thin film flip chip to the carrier wafer. The fabrication process includes 365-nm ultraviolet flip chip LED wafer align bonding with through-AlN-via wafer and sapphire laser lift-off. n-holes with the diameter of 100 µm were etched on the GaN epilayers for accessing n-type GaN. Through-AlN-via size was 110-µm and filled by Cu electroplating method for the electrical connection. Mechanical stabilization to prevent the GaN epilayers cracking and fragmentation during laser lift-off was achieved by utilizing epoxy based SU-8 photoresist support.

Cite

CITATION STYLE

APA

Kawan, A., & Yu, S. J. (2021). Laser Lift-Off of the Sapphire Substrate for Fabricating Through-AlN-Via Wafer Bonded Absorption Layer Removed Thin Film Ultraviolet Flip Chip LED. Transactions on Electrical and Electronic Materials, 22(2), 128–132. https://doi.org/10.1007/s42341-020-00273-1

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free