Abstract

A Ni/meso-MgO catalyst with high surface area and small Ni nanoparticles was synthesized and investigated for hydrogen production by steam reforming of phenol for the first time. Compared to conventional Ni/MgO, the Ni/meso-MgO catalyst showed higher catalytic activity and stability. X-ray Diffraction, N2 adsorption, hydrogen temperature programmed reduction, transmission electron microscopy and thermal gravimetry results indicated that the Ni/meso-MgO catalyst had higher surface area than Ni/MgO and Ni particles of Ni/meso-MgO were narrowly distributed in the range of 5~6 nm with an average size of 5.3 nm, while Ni particles of Ni/MgO were in the range of 6~10 nm with an average size of 7.92 nm. The small and uniform Ni nanoparticles in Ni/meso-MgO were attributed to the high surface area and the confinement effect of the mesoporous structure of meso-MgO, which could effectively limit the growth of the active metal and stabilize Ni particles during the procedure of NiO reduction. The mesoporous structure of Ni/meso-MgO also played an important role in suppressing Ni nanoparticle sintering and carbon deposition during the steam reforming of phenol reaction.

Cite

CITATION STYLE

APA

Yang, X., Wang, Y., & Wang, Y. (2015). Significantly improved catalytic performance of Ni-based MgO catalyst in steam reforming of phenol by inducing mesostructure. Catalysts, 5(4), 1721–1736. https://doi.org/10.3390/catal5041721

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free