Microstructure evolution and large magnetocaloric effect of La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 alloy prepared by strip-casting and annealing

8Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

This article is free to access.

Abstract

The microstructure and magnetocaloric effect of the La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 strip-cast flakes annealed between 1273K and 1423K for different time have been investigated. For the flakes annealed for 2h from 1273K to 1423K, the shape and distribution of α-Fe, La-rich and NaZn13-type 1:13 phases are quite sensitive to the annealing temperature. Especially, at a high annealing temperature of 1423K, the 1:13 phase began to decompose into macroscopic α-Fe conglomerations and La-rich dendrites. With the increase of annealing time from 0 to 12h at 1323K, the amount of 1:13 phase increased significantly and reached ∼93.50 wt.% at 12h. However, an overlong annealing time also led to 1:13 phase decomposition and influenced the magnetic performance. For the flakes annealed at 1323K for 12h, large magnetic entropy change value of 18.12Jkg-1K-1 at 5T has been obtained. The present results indicate that strip casting method can potentially be used in mass production of high performance magnetocaloric materials.

Cite

CITATION STYLE

APA

Zhong, X. C., Feng, X. L., Huang, J. H., Zhang, H., Huang, Y. L., Liu, Z. W., & Jiao, D. L. (2018). Microstructure evolution and large magnetocaloric effect of La0.8Ce0.2(Fe0.95Co0.05)11.8Si1.2 alloy prepared by strip-casting and annealing. AIP Advances, 8(4). https://doi.org/10.1063/1.4992057

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free