Abstract

Hot corrosion of Gas Tungsten Arc Welded (GTAW) AISI 304 and AISI 4140 dissimilar weldment exposed in air as well as molten salt environment of Na 2SO4-60%V2O5 and K 2SO4-60% NaCl are discussed. Weight gain studies were done for composite specimens containing both weld metal and heat-affected zone. The results indicated that the specimens were more corroded in molten salt environment as compared to air oxidation. Also weld interface of the samples showed more attack than base metals. © 2012 Springer-Verlag.

Cite

CITATION STYLE

APA

Arivazhagan, N., Devendranath Ramkumar, K., Karthikeyan, S., Manikandan, M., Narayanan, S., & Surendra, S. (2012). Hot corrosion studies on gas tungsten arc welded AISI 304 and AISI 4140 dissimilar joints. In Communications in Computer and Information Science (Vol. 330 CCIS, pp. 436–441). https://doi.org/10.1007/978-3-642-35197-6_48

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free