In vivo Wear Pattern of Experimental Composite Resins Containing Different Filler Components

5Citations
Citations of this article
17Readers
Mendeley users who have this article in their library.

Abstract

Using a scanning electron microscope (SEM) and an electron probe surface roughness analyzer (ERA), we conducted the in vivo study of the effect of various filler components on the wear of composite resins. Experimental light-cured composite resins were prepared employing three different filler components; -(1) Silica type, (2) Strontium type, and (3) Barium type. The filler content for all three types was 80 wt%,with the mean particlesize being 2.6 μm in diameter. The resin monomers consisted of 40 wt% Bis-GMA, 40 wt % TEGDMA and 20 wt% UTMA. These materials were placed in 2 mm diameter cylindrical cavities located in the OCA (occlusal contact area) or the CFA (contact free area) of cast crowns temporarily set in a volunteer patient's mouth. The crowns were removed at monthly intervals for longitudinal SEM observation. After two months, worn surfaces were also analyzed by ERA. The result showed that the wear patterns of the composites were characterized by the filler components, especially in the OCA. © 1994, The Japanese Society for Dental Materials and Devices. All rights reserved.

Author supplied keywords

Cite

CITATION STYLE

APA

Sekiya, K., Okamoto, A., Fukushima, M., & Iwaku, M. (1994). In vivo Wear Pattern of Experimental Composite Resins Containing Different Filler Components. Dental Materials Journal, 13(1), 36–46124. https://doi.org/10.4012/dmj.13.36

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free