Biodegradation and non-enzymatic hydrolysis of poly(Lactic-co-glycolic acid) (plga12/88 and plga6/94)

14Citations
Citations of this article
43Readers
Mendeley users who have this article in their library.

Abstract

The predicted growth in plastic demand and the targets for global CO2 emission reduc-tions require a transition to replace fossil-based feedstock for polymers and a transition to close-loop recyclable, and in some cases to, biodegradable polymers. The global crisis in terms of plastic littering will furthermore force a transition towards materials that will not linger in nature but will degrade over time in case they inadvertently end up in nature. Efficient systems for studying polymer (bio)degradation are therefore required. In this research, the Respicond parallel respirometer was applied to polyester degradation studies. Two poly(lactic-co-glycolic acid) copolyesters (PLGA12/88 and PLGA6/94) were tested and shown to mineralise faster than cellulose over 53 days at 25 °C in soil: 37% biodegradation for PLGA12/88, 53% for PLGA6/94, and 30% for cellulose. The corresponding monomers mineralised much faster than the polymers. The methodology presented in this article makes (bio)degradability studies as part of a materials development process econom-ical and, at the same time, time-efficient and of high scientific quality. Additionally, PLGA12/88 and PLGA6/94 were shown to non-enzymatically hydrolyse in water at similar rates, which is relevant for both soil and marine (bio)degradability.

Cite

CITATION STYLE

APA

Wang, Y., Murcia Valderrama, M. A., van Putten, R. J., Davey, C. J. E., Tietema, A., Parsons, J. R., … Gruter, G. J. M. (2022). Biodegradation and non-enzymatic hydrolysis of poly(Lactic-co-glycolic acid) (plga12/88 and plga6/94). Polymers, 14(1). https://doi.org/10.3390/polym14010015

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free