The reduction in uniaxial compressive strength (UCS) was investigated for sandstones under various moisture levels. Thirty-four UK Darney sandstone samples were tested under six different moisture conditions. The time-dependent moisture gain and loss were also evaluated. For 77 sandstones identified in the literature, the loss of UCS between oven-dry and saturated conditions was up to 45%, with an average of 20%. For Darney stone, the average loss of UCS was around 20%, with UCS around 72 N/mm2 when oven-dry and 58 N/mm2 when fully saturated. During saturation, significant loss of UCS occurred soon after exposure to water with 80% of UCS being lost within the first 2.5–6 hours. For Darney stone 50% of UCS was lost at air-dry conditions. Results from the 78 sandstone types were compared with the equivalent compressive strength defined by BS EN 772–1:2011 for oven-dry, air-dry, and saturated conditions. The estimated values by BS EN 772–1:2011 for dry and saturated UCS agreed well with the available test data and indicated a lower-bound solution. For immersed conditions, BS EN 772–1:2011, however, overestimates the reduction in UCS for a large number of samples and provides an average, instead of a lower-bound solution.
CITATION STYLE
Tomor, A. K., Nichols, J. M., & Orbán, Z. (2024). Evaluation of the Loss of Uniaxial Compressive Strength of Sandstones Due to Moisture. International Journal of Architectural Heritage, 18(5), 771–787. https://doi.org/10.1080/15583058.2023.2188313
Mendeley helps you to discover research relevant for your work.