In the current study, effect of SiO2/Na2O ratio in Sodium silicate (Na2SiO3) solution, Na2SiO3/NaOH ratio and molarity of NaOH on the compressive strength of geopolymer concrete. A geopolymer mix design is formulated with various mixes are casted with alkali activator solution (AAS)/fly ash (FA) =0.5 and constant fly ash content. The molar ratio of SiO2/Na2O in Na2SiO3 solution is altered from 1.50 to 3.00 for different ratios of Na2SiO3/NaOH (2.0, 2.5 and 3.0) and also for various molarities of NaOH (8M,10M,12M,14M,16M and 18M) are studied for their synergic effect on the compressive strength of geopolymer concrete. Results highlighted that the 16M NaOH yields high compressive strength when SiO2/Na2O in Na2SiO3 solution is around 2.00 to 2.40 and Na2SiO3/NaOH=2.5.

Cite

CITATION STYLE

APA

Srinivasa Reddy, V., Krishna, K. V., Rao, M. V. S., & Shrihari, S. (2021). Effect of molarity of sodium hydroxide and molar ratio of alkaline activator solution on the strength development of geopolymer concrete. In E3S Web of Conferences (Vol. 309). EDP Sciences. https://doi.org/10.1051/e3sconf/202130901058

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free