Annealing of amorphous Sm5Fe17 melt-spun ribbon

5Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

An amorphous Sm5Fe17 melt-spun ribbon was annealed under various conditions to obtain the metastable Sm5Fe17 phase. The Sm5Fe17 phase could be obtained by annealing at temperatures between 873 K and 973 K for 0.1-1 h. However, the annealed specimens contained other phases such as the SmFe2 and SmFe 3 phases depending on the annealing conditions. It was found that the specimen annealed at 873 K for 1 h consisted mostly of the Sm 5Fe17 phase. The Sm5Fe17 phase could also be obtained by annealing the amorphous Sm5Fe17 melt-spun ribbon at 1073 K for 0.1 h or 0.3 h, but annealing at that temperature for 1 h resulted in decomposition of the metastable Sm5Fe 17 phase and formed the equilibrium Sm2Fe17 and SmFe3 phases. © 2008 The Japan Institute of Metals.

Cite

CITATION STYLE

APA

Saito, T. (2008). Annealing of amorphous Sm5Fe17 melt-spun ribbon. Materials Transactions, 49(6), 1446–1450. https://doi.org/10.2320/matertrans.MBW200781

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free