Electrical resistivity and thermal conductivity of W and Re up to 5 GPa and 2300 K

11Citations
Citations of this article
12Readers
Mendeley users who have this article in their library.
Get full text

Abstract

The electrical resistivity of solid-state tungsten (W) and rhenium (Re) was experimentally measured at high pressures up to 5 GPa and temperatures up to ∼2273 K using a four-wire resistivity method. For both metals, the resistivity decreased as a function of pressure and increased as a function of temperature, in excellent agreement with 1 atm data. The Wiedemann-Franz law was used to calculate the total thermal conductivity from the resistivity. Thermal conductivity increased as a function of pressure for both metals, but decreased as a function of temperature for W and increased for Re. Values of thermal conductivity at high pressures and temperatures are consistent with most recommended previous experimental studies at 1 atm.

Cite

CITATION STYLE

APA

Littleton, J. A. H., Secco, R. A., Yong, W., & Berrada, M. (2019). Electrical resistivity and thermal conductivity of W and Re up to 5 GPa and 2300 K. Journal of Applied Physics, 125(13). https://doi.org/10.1063/1.5066103

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free