Effect of Quench Tempering on Hydrogen Embrittlement and Corrosion Behavior of X100 Pipeline Steel

11Citations
Citations of this article
7Readers
Mendeley users who have this article in their library.

Abstract

In this study, the hydrogen embrittlement and corrosion behavior of X100 pipeline steel (Ref) was investigated after various heat treatments, including one-step austenitizing at 880 °C (HT3), 830 °C (HT2), and 780 °C (HT1) for 90 min, oil quenching to room temperature, tempering at 600 °C for 30 min, and air cooling to room temperature. Potentiodynamic polarisation was performed to assess the electrochemical corrosion behavior, while the Charpy impact test and Vickers microhardness measurement were performed to assess the hydrogen embrittlement susceptibility before and after hydrogen charging. SEM, EBSD, and EDS were used to further characterize the fractured surface and crystallographic texture of specimens, while XRD was used to evaluate the macro-texture and corrosion products. The results of the Charpy impact and hardness tests showed that the high hardness and low impact energy values in the Reference and HT3 specimens were linked to a higher susceptibility to hydrogen embrittlement, indicating that the hardness values and Charpy impact energy, respectively, increased and decreased with a decrease in the hydrogen embrittlement resistance. The micro-texture results from the EBSD analysis showed that the HT3 and Ref. specimens had higher Kernel average misorientation (KAM) values and higher deformed grains fractions than those of the HT2 and HT1 specimens, resulting in lower corrosion resistance. The HT2 specimen had an optimal combination of beneficial ({110}, {111}, {332}) and harmful texture components ({100}), showing that corrosion resistance can be improved.

References Powered by Scopus

Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking

329Citations
N/AReaders
Get full text

Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel

243Citations
N/AReaders
Get full text

Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking

194Citations
N/AReaders
Get full text

Cited by Powered by Scopus

An experimental and statistical study on the characteristics of non-metallic inclusions that serve as hydrogen-induced crack nucleation sites in pipeline steel

21Citations
N/AReaders
Get full text

Experimental observations of nucleation and crack growth paths of hydrogen-induced cracking in pipeline steel

15Citations
N/AReaders
Get full text

Effect of Electrochemical Hydrogen Charging on Hydrogen Embrittlement and Mechanical Properties of Quenched Tempered X100 Pipeline Steel

5Citations
N/AReaders
Get full text

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Cite

CITATION STYLE

APA

Khatib Zadeh Davani, R., Mohtadi-Bonab, M. A., Yadav, S., Entezari, E., Cabezas, J. F. A., & Szpunar, J. (2023). Effect of Quench Tempering on Hydrogen Embrittlement and Corrosion Behavior of X100 Pipeline Steel. Metals, 13(5). https://doi.org/10.3390/met13050841

Readers over time

‘23‘2402468

Readers' Seniority

Tooltip

PhD / Post grad / Masters / Doc 4

100%

Readers' Discipline

Tooltip

Engineering 1

50%

Materials Science 1

50%

Article Metrics

Tooltip
Mentions
Blog Mentions: 1
News Mentions: 1

Save time finding and organizing research with Mendeley

Sign up for free
0