Mechanical properties of composites with titanium diboride fabricated by spark plasma sintering

2Citations
Citations of this article
6Readers
Mendeley users who have this article in their library.

Abstract

Microstructure and mechanical properties of the 316L steel composite reinforced with TiB2 phase were examined. The test materials were obtained by SPS technique from powders. From testing of the mechanical properties it follows that the optimum temperature for the fabrication of 316Lsteel-TiB2 composites by SPS is 1100°C. Studies have also proved that the critical content of TiB2 phase in steel matrix should not exceed 6vol%. Above this level, the plastic properties of the composite become unstable and strongly dependent on the time of sintering.

Cite

CITATION STYLE

APA

Sulima, I., Boczkal, G., & Palka, P. (2017). Mechanical properties of composites with titanium diboride fabricated by spark plasma sintering. Archives of Metallurgy and Materials, 62(3), 1665–1671. https://doi.org/10.1515/amm-2017-0255

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free