The aim of this study was to investigate the impact of the addition of a minor quantity of Si on the microstructure evolution, heat treatment response, and mechanical properties of the Al–4.5Cu–0.15Ti–3.0Mg alloy. The microstructure analysis of the base alloy revealed the presence of α-Al grains, eutectic α-Al-Al2CuMg (S) phases, and Mg32(Al, Cu)49 (T) phases within the Al grains. In contrast, the Si-added alloy featured the eutectic α-Al-Mg2Si phases, eutectic α-Al-S-Mg2Si, and Ti-Si-based intermetallic compounds in addition to the aforementioned phases. The study found that the Si-added alloy had a greater quantity of T phase in comparison to the base alloy, which was attributed to the promotion of T phase precipitation facilitated by the inclusion of Si. Additionally, Si facilitated the formation of S phase during aging treatment, thereby accelerating the precipitation-hardening response of the Si-added alloy. The as-cast temper of the base alloy displayed a yield strength of roughly 153 MPa, which increased to 170 MPa in the Si-added alloy. As a result of the aging treatment, both alloys exhibited a notable increase in tensile strength, which was ascribed to the precipitation of S phases. In the T6 temper, the base alloy exhibited a yield strength of 270 MPa, while the Si-added alloy exhibited a significantly higher yield strength of 324 MPa. This novel Si-added alloy demonstrated superior tensile properties compared to many commercially available high-Mg-added Al–Cu–Mg alloys, making it a potential replacement for such alloys in various applications within the aerospace and automotive industries.
CITATION STYLE
Shah, A. W., Ha, S. H., Siddique, J. A., Kim, B. H., Yoon, Y. O., Lim, H. K., & Kim, S. K. (2023). Microstructure Evolution and Mechanical Properties of Al–Cu–Mg Alloys with Si Addition. Materials, 16(7). https://doi.org/10.3390/ma16072783
Mendeley helps you to discover research relevant for your work.