Push-out bond strength of root-end filling materials

11Citations
Citations of this article
45Readers
Mendeley users who have this article in their library.

Abstract

The aim of this study was to evaluate the bond strength of root-end filling materials. Forty 2-mm-thick slices were obtained from human single-rooted teeth. After root canal preparation using a 1.5 mm diameter cylindrical drill, the dentinal walls were prepared by diamond ultrasonic tip (CVD T0F-2). The specimens were divided according the material (n=10): MTA Angelus (MTAA), MTA Sealer (MTAS, experimental), Sealer 26 (S26) and zinc oxide and eugenol cement (ZOE). The push-out test was performed in a mechanical test machine (EMIC DL 2000) at 1 mm/min speed. The failure type was evaluated by stereomicroscopy. The results were subjected to ANOVA and Tukey test, at 5% significance level. MTAA (19.18 MPa), MTAS (19.13 MPa) and S26 (15.91 MPa) showed higher bond strength (p<0.05). ZOE (9.50 MPa) showed the least bond strength values (p<0.05). Adhesive failure was prevalent in all groups, except for ZOE, which showed mixed failures. It was concluded that root-end filling materials MTA Angelus, MTA Sealer and Sealer 26 showed higher bond strength to dentinal walls than zinc oxide and eugenol cement after retrograde preparation.

Cite

CITATION STYLE

APA

Vivan, R. R., Guerreiro-Tanomaru, J. M., Bosso-Martelo, R., Costa, B. C., Duarte, M. A. H., & Tanomaru-Filho, M. (2016). Push-out bond strength of root-end filling materials. Brazilian Dental Journal, 27(3), 332–335. https://doi.org/10.1590/0103-6440201600340

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free