Atomic layer deposition in nanostructured photovoltaics: tuning optical, electronic and surface properties

  • Palmstrom A
  • Santra P
  • Bent S
  • 54


    Mendeley users who have this article in their library.
  • 23


    Citations of this article.


This review highlights applications of atomic layer deposition for third generation photovoltaics, including light absorption, barrier layer formation and passivation.