Plasma-enhanced atomic layer deposition of Co using Co(MeCp)2 precursor

28Citations
Citations of this article
46Readers
Mendeley users who have this article in their library.
Get full text

Abstract

Cobalt (Co) thermal or plasma enhanced atomic layer deposition (PE-ALD)was investigated using a novel metal organic precursor, Co(MeCp)2, and NH3 or H2 or their plasma as a reactant. The growth characteristics, electrical and microstructural properties were investigated. Especially, PE-ALD produced Co thin films at low growth temperature down to 100 °C. Interestingly, the low temperature growth of Co films showed the formation of columnar structure at substrate temperature below 300 °C. The growth characteristics and films properties of PE-ALD Co using bis(η-methylcyclopentadienyl) Co(II) (Co(MeCp)2) was compared with those of PE-ALD Co using other Cp based metal organic precursors, bis-cyclopentadienyl cobalt (II) (CoCp2) and cyclopentadienyl isopropyl acetamidinato-cobalt (Co(CpAMD)). Copyright © 2013, Dalian Institute of Chemical Physics, Chinese Academy of Sciences.

Cite

CITATION STYLE

APA

Park, J., Lee, H. B. R., Kim, D., Yoon, J., Lansalot, C., Gatineau, J., … Kim, H. (2013). Plasma-enhanced atomic layer deposition of Co using Co(MeCp)2 precursor. Journal of Energy Chemistry, 22(3), 403–407. https://doi.org/10.1016/S2095-4956(13)60052-2

Register to see more suggestions

Mendeley helps you to discover research relevant for your work.

Already have an account?

Save time finding and organizing research with Mendeley

Sign up for free