Abstract
Effective method for preventing sigma phase embrittlement in Ni-base superalloys by altering composition slightly; stress-rupture and creep are also influenced by composition change.
Author supplied keywords
Cite
CITATION STYLE
APA
Boesch, W. J., & Slaney, J. S. (1964). Preventing sigma phase embrittlement in nickel base superalloys. Metal Progress, 86(1), 109–111.