Abstract
Were studied. The capacity change observed for carbon samples after storage at elevated temperatures is attributed to the instability of the SEI layer in the liquid electrolyte. The capacity change was found to correlate well with the specific surface area of graphite.
Cite
CITATION STYLE
APA
Zheng, T., Gozdz, A. S., & Amatucci, G. G. (1999). Reactivity of the Solid Electrolyte Interface on Carbon Electrodes at Elevated Temperatures. Journal of The Electrochemical Society, 146(11), 4014–4018. https://doi.org/10.1149/1.1392585