Abstract
The research that has been carried out on the photosonolytic degradation of methyl red uses a ZnO as a catalyst which aims to determine the effect of time and catalyst mass on the degradation of methyl red. The time of degradation is about 30 to 150 minutes while about 0,05 grams to 2,5 grams of catalyst mass is used. The measurement results of the Uv-Vis spectrophotometer were obtained at a wavelength of 435nm with an absorbance 0,2471. In the variation of the degradation time, the highest result was obtained at 60 minutes which was 75,27%. This study shown that hydroxyl radicals (∙OH) takes as a main control in degrading of methyl red.
Cite
CITATION STYLE
Ayu, P., Putra, A., Sanjaya, H., Dewata, I., & Yohandri, Y. (2021). Degradasi Zat Warna Metil Merah Dengan Katalis ZnO Menggunakan Metode Fotosonolisis. Jurnal Periodic Jurusan Kimia UNP, 10(2), 56. https://doi.org/10.24036/p.v10i2.112453